ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 2,
Visits: 13
I am trying to cast small helical gears from a gearbox we use. I am using the Easy Composites Starter kit. Frst timer
I have tried using FAST CAST Polyurethane Casting Resin, with mixed results, though still testing. My question is, the originals appear to be a form of nylon. Is there different materials available to cast with other than FAST CAST, that have properties that are closer to nylon. Also is there other materials that are easier to pour or are closer to water.
Best Regards
Carltonm
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Nylon Gears
Carltonm
-
14 Years Ago
Hi Carltonm, When you say you're getting 'mixed results' using the Fast-Cast, can you elabourate on...
Matt (Staff)
-
14 Years Ago
Dear Matt Thanks for coming back to me. The main problem I have had is small air bubbles at the...
Carltonm
-
14 Years Ago
Hi Carlton, Sorry for the delay in getting back to you. I see, given the tiny scale you're working...
Matt (Staff)
-
14 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search