Clear high temperatur epoxy


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In terms of high temperature casting resins, unfortunately we do not have anything that will go up to that temperature.  The GlassCast range of resins are limited to around 50C HDT. I am yet to find a high temperature clear casting resin system that is clear.  Higher temperature resins, due to the additives needed, tend to be quite amber in colour which is highly undesirable in most clear casting applications.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
RasmusT
R
Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)Junior Member (13 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hi,
I working on a project where we will mould LED lights into epoxy. The surface of the LED can reach temperature at 150 deg C. I`m looking for clear/tranparent epoyx that can handle the high temperature.

Do not hesitate to contact me if you have questions

Vennlig hilsen
Rasmus Tørnqvist
Senior Mechanical Engineer
INNOVA AS
Jakob Askelandsvei 13
N-4314 SANDNES
Mob: 473 48 559
Skype for business

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search