Greetings,

I recently did some repairs on my mould and after some sanding down, applied a layer of gelcoat with the wax additive included. Today, I decided to clean the mould with the Easy Lease mould cleaner in preparation for the release agent before doing some resin infusion.
However, I noticed the gelcoat getting tacky again with every swipe of the cloth and stopped. So my question, has anyone else experienced this?
Is the mould cleaner acting like a thinner and eroding the wax additive?