I’ve been using Glasscast 3 for quite a while now with no problems at all, but today I did something wrong but not sure what. I sometimes warm the resin in water if I want it to be more fluid, today I may have left it to warm for too long. Would this cause the resin to cure too quickly and get hot? The pour looks ok at the moment, but will it cure properly?