	Group: Forum Members 	        
    Posts: 99, 
    Visits: 676 
    
 
          
		     | 
				                       
                 
                
                    
			            I’m sure this has been covered and I searched but what I found of others asking had no answers. Then I google searched and just got how to kill mold in your house lol. I have a part that was primed with Spies Hecker 5310 HS primer. If I block this out and work my way to finer grits, can I use this as the plug surface to make a mold? Or should I paint and clear, polish and buff it to get a good surface. I’m worried the primer will be too porous.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |