Anyone know how to get rid of bubbles. They’re so small and are filled white from wet sanding and polishing. You can’t feel them with your fingernail. I’ve tried white spirit but no luck.
This is glasscast 3 on top of glasscast 50
I don’t want to resand the table. Just hoping there’s a product I can clean it with