Mixing Solution MW Wax Gelcoat Additive


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
First of all, we always recommend ignoring the solution mw when calculating the catalyst ratio.  You are only catalysing the actual gelcoat or resin, not the additives.

Typically you use Solution MW at around 2% by weight.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Kevin254
K
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 4, Visits: 15
I am doing some minor repairs on my mould. I wanted to know in what ratios the MW wax is added to the Gelcoat. For example, how much of the wax is added to 100gms of gelcoat?
Additionally, when calculating how much MEKP to use, do I factor in the new weight of the gelcoat+ wax?

Thanks.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search