I’m very new to the world of epoxy resin and I’m stumbling along learning with each project I do, I’ve tried making a few small coasters with glass cast 10/50 and your metallic pigments, the problem I’m having is that the metallic particles are settling as the resin hardens and spoiling the amazing effect they have when you first pour them, do you have any suggestions before I move onto bigger projects?