Bonobo
Bonobo
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Following on from my previous thread in "Pattern and plugmaking"
http://www.talkcomposites.com/623/Pattern-Making-and-CAD,-need-advice
in which you can see the design and pattern making of this spoiler
My plug is now nearly ready
I'm now thinking about how to make the mould, i'm considering making a 2 part split mould as illustrated cross section below, i haven't done this before so please add your comments on how you think it would work out or how i can do it better.
what would be the best material to use for the barriers?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Looking for best way to make this mould
Bonobo
-
14 Years Ago
Ok, my reason for a two part mold is the undercut, i put an undercut where the spoiler meets the...
Bonobo
-
14 Years Ago
Nice work you are doing. There are a number of ways to make your flanges. I have used plasticine,...
fgayford
-
14 Years Ago
Thanks for the feedback Fred, i'm at the stage now of flatting and polishing the plug. I've got...
Bonobo
-
14 Years Ago
Plug polished up with release agent and wax
Bonobo
-
13 Years Ago
whoa! i have the EXACT same issue! i have a foha spoiler for my 87 bmw 325 that is long out of...
brasco
-
13 Years Ago
[quote][b]brasco (11/01/2013)[/b][hr]whoa! i have the EXACT same issue! i have a foha spoiler for my...
Bonobo
-
13 Years Ago
started making the mould now, backing up with CSM and polyester resin. next step will be to make the...
Bonobo
-
13 Years Ago
What kind of 2k filler primer did you use? I've heard of using both polyester and urethane. Does one...
SRM
-
10 Years Ago
Not really, I've used both and they are quite much of a muchness. It's not the base resin that makes...
Hanaldo
-
10 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search