Group: Forum Members
Posts: 24,
Visits: 69
|
Hi group!, there is a way to reduce the Gardner color of an amine hardener? I would like to use this hardener to cast over wood, and the current resulting color of the mix (2:1 epoxy clar resin:hardener) is almost orange. There is a reagent or something could be used to clear the color of the hardener.?, just the orange color to pale amber
|