I have found one on-line vendor offering UV inhibitor, but the video tutorials that are available do not discuss the need for any added step to protect carbon fiber products. Will the resin used in all three methods of Carbon Fiber fabrication (Resin Infusion, Hand Layup, and Prepreg) have UV inhibitors included in the resin chemistry?