Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As long as the resin is fully cured, then generally a clean microfibre cloth with remove finger print marks and loose dirt.  Any more stubborn marks should come off with warm soapy water.  Be careful to rinse and dry properly so you get no drying marks.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Black Knight
B
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 1, Visits: 43
I have castings made from mostly smooth on 300 resin and they are getting dirty from handling etc. Is there a recommended way of cleaning this material or resin general without harming the object?