PET is typically a low reactivity plastic and we would not expect the resin to stick to it.  PETG is a co-polymer of PET so should share similar properties, however we have not specifically tested PETG ourselves so cannot be 100% sure it will ok.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Omega
O
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 56
Hi
 Does epoxy resin such as Clearcast 50 adhere to Polyethylene Terephthalate Glycol (PETG)  clear 2mm sheet ? or would a release agent be required?

I know you supply Polypropylene Sheet for this  but need to know if PETG has the same release properties.
thanks 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search