Mindaugas Skorupskas
Mindaugas Skorupskas
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 12
Hi
I have mixed Pearl ex metalic powder with isopropyl alcohol, but spray bottle keeps clogging. Any idea what has went wrong?
Edited
7 Years Ago by
Mindaugas Skorupskas
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pearl ex metalic pigments
Mindaugas Skorupskas
-
7 Years Ago
The pigments have quite a large solid content in quite a large particle size so I suspect it is just mechanically clogging the bottle. Try a bigger nozzle if possible.
Warren (Staff)
-
7 Years Ago
Thanks for the reply. I had adjustable nozzle spray bottle for £2. Bought an expensive spry bottle and now it works.
Mindaugas Skorupskas
-
7 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search