It sounds like you have a small leak somewhere. You should be able to achieve fully leak tight bags with the material. Running the pump against a tiny leak is not going to cause any issues with the pump and is fine from a gluing down perspective.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
meiros
meiros
Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)
Group: Forum Members
Posts: 1, Visits: 17
Hi everyone,
Last year I bought the below equipment to laminat wood in vacuum bags:

VP425 Composites Vacuum Pump
TBC2 Through-Bag Connector
VB160 Vacuum Bagging Film 1.52m LFT 
Vacuum Bagging Gum Sealant Tape 15m Rolls
1/4 Turn Vacuum Valve
6mm Hose-Tail Barb Connector
6mm ID Budget PVC Vacuum Hose 5m

I could not make a good vacuum bag to keep the wood pressed during gluing process.
I made the bag carefully to make sure it was well sealed but the truth is that it never stays. I can make vacuum, but when I turn off the pump or close the valve, the bag loses its vacuum.
The glue has to dry about 3 hours. Should I leave the pump on during 3 hours?
But should not he be able to turn off the pump as soon as the vacuum was set?
Thank you