+x make_pr - 12/9/2018 1:59:05 PMI am casting a large section in a silicone mould using Glasscast 50 and then sanding the open surface back. I want to have a clear, glossy and flat coating on top then.Is it possible to use Glasscast 3 as a thin coating on top of Glasscast 50 to achieve this ?Is there any other method which would achieve the effect ?
+x Matthieu Libeert - 12/9/2018 10:12:08 PM+x make_pr - 12/9/2018 1:59:05 PMI am casting a large section in a silicone mould using Glasscast 50 and then sanding the open surface back. I want to have a clear, glossy and flat coating on top then.Is it possible to use Glasscast 3 as a thin coating on top of Glasscast 50 to achieve this ?Is there any other method which would achieve the effect ?Glasscast 3 worked for me as a "flow coat" to achieve a gloss finish after sanding the glasscast 50