My oven was 20c higher than the setting on the pid controller when tested with a stand alone k type probe ' which is the best k type probes to use on these ovens please 
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
That seems quite a high discrepancy, but did you allow some time for the oven temperature to even out? If the built-in probe is at the top of the oven, for instance, then the part temperature can take some time to read the same if it's sitting lower down. 

It's sometimes worth using a portable probe as a matter of course that has a couple of long string-like probes that you can stick to the part and use this device to reliably assess part temperature, especially in the early stages of a heating cycle


Barnsley-Bill
B
Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)Supreme Being (212 reputation)
Group: Forum Members
Posts: 25, Visits: 489
MarkMK - 12/7/2018 8:21:54 AM
That seems quite a high discrepancy, but did you allow some time for the oven temperature to even out? If the built-in probe is at the top of the oven, for instance, then the part temperature can take some time to read the same if it's sitting lower down. 

It's sometimes worth using a portable probe as a matter of course that has a couple of long string-like probes that you can stick to the part and use this device to reliably assess part temperature, especially in the early stages of a heating cycle


It was while ramping up to 120c for 3 hours on the final cure of the mould ' the k type probe I have are the stick on type but I might try some others just asking what type do other members use.
Thanks

supanova
supanova
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 3, Visits: 19
I find there is normally a bit of difference from what my thermo reads and the air temp of the oven. Any where between 6 and 22 degrees.
I do put the thermo in the vac bag, taped to the mould.  I use the exposed junction thermocouples. I wouldn't worry about it to much.
(Apologies if I've got the wrong end of the stick).
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search