Hello,

So, I have broken carbon fiber longboard and planning to repair it. I have no experience, so would appreciate your help.

1) Which Carbon fiber cloth to choose? (keep in mind it should hold high weight pressure)
2) Which epoxy resin to use? (keep in mind it should hold high weight pressure)
3) Where to start?

I will try to remove a bit of old (broken) carbon fiber layers and do some polishing to eliminate sharp edges.
Next I am planning to apply a thin layer of epoxy resin and let it dry (to strengthen broken layers which will remain on the board).
Next I am planning to add new carbon fiber layers, glue it with epoxy resin and let it dry.

Would you do it the same way?
Any advices?
Do I need to use vacuum bag?

Thank you in advance for your help Smile 