EB700 High Temperature Epoxy Tooling Board


Author
Message
gbone
g
Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)
Group: Forum Members
Posts: 1, Visits: 5
In the data sheet for EB700  it gives a working temp of 130deg.

I would like to know if this board is OK to use in an Autoclave with Pre-Pregs needing a  Curing temp of 142 degs ???  

Plus, do you always have  to seal the board. I am only looking to make 3-4 parts