Frank
Frank
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 27,
Visits: 123
Hello
I need to cut Carbon Fibre 2/2 Twill 3k 210g in 45°.
The method with the pulled strand does not work here.
It ist for my project:
carbon front fender 701 supermoto
I added some pictures at the end.
Any hints?
regards
Frank
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cutting Carbon Fibre 45°
oberflaeche
-
8 Years Ago
Do you mean cutting strips or ply shapes at 45degrees? Get a triangle or make one and use as a guide for cutting at 45 degrees
scottracing
-
8 Years Ago
But I cut with scissors and so I have to lift up the weave a little bit. By lifting it up, it is difficult to hold the template in place. I could mark it with spray color or something or cut it layin...
oberflaeche
-
8 Years Ago
get a fabric cutting mat and rotary pizza fabric cutter
George Sychrovsky
-
8 Years Ago
Thank you. i will try a pizza cutter... Frank
oberflaeche
-
8 Years Ago
Dont use a pizza cutter, use a fabric rotary cutter. Looks like a pizza cutter but they are much sharper and better quality.
Hanaldo
-
8 Years Ago
Ok, I will try a Rotary Cutter 60mm from fiskars. Thank you Frank
oberflaeche
-
8 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search