scottracing - 11/27/2018 9:50:04 PM
i would have a search over on the FSAE forums for foam attenuators, as a lot of the teams use foam for the job.

When i dont FS many moons ago we used a closed cell rohacell, i cant remember the density but it done the job. Have a look at the latest formula student regulations and they should give you a starter for 10. Also have alook on some of the rohacell  seller sites like Emkay Plastics


Ah perfect thanks! Will have a dig Smile

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
i would have a search over on the FSAE forums for foam attenuators, as a lot of the teams use foam for the job.

When i dont FS many moons ago we used a closed cell rohacell, i cant remember the density but it done the job. Have a look at the latest formula student regulations and they should give you a starter for 10. Also have alook on some of the rohacell  seller sites like Emkay Plastics


mowgli
m
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 10
Hello folks, newbie here!

I am currently researching energy attenuation methods for use in blast mitigation (MEng project), and have been struggling to find data for foams.
I understand the vast variance in foams makes this difficult, but I wondered if anyone has any information or experience which they could share with regards to using foam to attenuate energy in a crash situation?

Any info would be fab, and any other possible suggestions welcome!

Cheers, Morgan