Group: Forum Members
Posts: 6,
Visits: 49
|
Welcome. This is my first attempt with these products. I have a few questions: First What you use to activate a Epoxy Polyester Gelcoat Compatible to the carbon fibre cloth adhere to the surface?
Second in Part film about the creation of Carbon Fibre bonnet, specifically the underside of parts what you used for positioning cloth? what kind of spray? Do you have this for sale?
Thank you and best regards
|