Hi, I want to make 2 front wings in carbon for my 106 Maxi and I have the original items to make a mould from.

I have no doubt if I had all the stuff in front of me I could make a panel I would be happy with but I get

totally lost when I try to figure out what exactly I need to make a mould and what I need to make the carbon

panel and how much of everything is required.

I am not looking for a smooth show finish as the panels will be painted and covered in sign wrighting so

do I need to vacuum bag them of is there another way around it.

Thanks in advance for your help.