Varnishing resin on a river table


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can varnish the resin if you so desire - depending on the resin adhering properly, however there is usually no need as the GlassCast 50 can be polished to a high gloss in its own right.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
Table ready to varnish so varnished the wood and the resin.
Not overly happy with how it came out so have had to sand it all the way back down now and will have to work back up thru the grits.
Thinking of just varnishing the wood and avoiding the resin.
I thought it was ok to varnish resin though?
Using glasscast 10/50