Keep in mind that alginate is a water based product, and is actually only useable for a couple of hours while it is still very wet. Theres a lot of resins that wont like being poured into that, especially polyurethanes. Epoxies might cope, but depends on the specific epoxy, theres a good chance they will absorb water and come out very milky. 


The ideal solution is to use a skin safe silicone instead of the alginate, but this will be significantly more expensive, especially for a one off project.
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In Essence, you would take a mould from the part you have made then use the mould to cold cast the finished item with a metal powder of your choice.

This video is exactly the kind of process you would do for your project:




Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 8 Years Ago by Warren (Staff)
mark vr
mark vr
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 1, Visits: 5
I'd like to use something like this:
https://www.amazon.co.uk/Baby-Chromatic-Alginate-Moulding-Powder/dp/B071GPRGDF
To cold cast some body parts with metal powder.

What would be the best resin/epoxy etc to use?

Thanks!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search