			            We recommend a 2 bucket method, mixing in the first bucket for 5 mins before pouring into a second and mixing for another 5 mins.  That way you minimise the chances of any unmixed or poorly mixed resin making its way onto the resin. 
 If you aren't bonding legs into place (such as large end legs like in our video,), then you can screw into the wood for the best support.  Resin on its own is much like most plastics and unlikely to make a strong thread.
 
 