			            Good morning all,
 I'm new to the casting game, and am looking for some advice!
 
 The plan is to cast a cylindrical part roughly 25mm in diameter and 80mm in height, and want it to be as clear as possible.
 
 Mould wise I am considering one of the Smooth-On silicon products (Mould Star or SORTA-Clear).
 
 Casting resin I'm considering GlassCast 50 (based on the total height of the part).
 
 I do not have degassing/vacuum kit available.
 
 I have been reading around, trying to ensure I'm selecting compatible materials etc., but figured it safest to ask the community!
 