Group: Forum Members
Posts: 408,
Visits: 4.1K
|
Similar to wet lay, as there is no heat involved :-)
Personally, I would just add 4-6 layers of fibreglass to the back of the mould and a 30-40mm high lip around the edge to add additional stiffening to this area. Do this with the mould in the pattern.
|