Hi everyone, I am a backyard surfboards shaper who wants to move the first steps in the vacuum bagging world, to make composite surfboards-kiteboards-sups.I have no idea where to start from in terms of gear needed, vacuum bagging techniques etc.Could any of you please suggest me a section of this forum where I can gather all these infos?Thanks.
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
fishbone_surfboards - 9/12/2018 9:43:25 AM
Hi everyone, I am a backyard surfboards shaper who wants to move the first steps in the vacuum bagging world, to make composite surfboards-kiteboards-sups.I have no idea where to start from in terms of gear needed, vacuum bagging techniques etc.Could any of you please suggest me a section of this forum where I can gather all these infos?Thanks.

Watch all of the tutorial videos on the Easycomposites page for a good grounding in composite techniques.

https://www.easycomposites.co.uk/learning