Matthieu Libeert
Matthieu Libeert
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I'm planning to make a silicone vacuumbag for infusion.
I see you are selling
Fumed Colloidal Silica
to make a more thixotrope RESIN.
Is it possible to add it to Silicone too?
I want to make a silicone vacuumbag but I'm scared that if I brush the silicone onto the mould it will all drip off the sides and
all fall down to the deepest point of the mould.
Would this help to keep it better sticking to the sides of the mould or do you advice an other additive to the silicone?
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fumed Colloidal Silica and Silicone
matthieutje65
-
14 Years Ago
Hi Matthieu, Colloidal silica would not be suitable to add to silicone to make it 'brushable' -...
Matt (Staff)
-
14 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search