Group: Forum Members
Posts: 408,
Visits: 4.1K
|
I assume that you laid the carbon on the 'gel coat' dry? You need to thoroughly soak the carbon otherwise this can happen.
On the gel coat issue, why are you adding one? If the mould is shiny and you are using a chemical release agent, such as Easy Lease, then the carbon will come out shiny. Brush on a light coat of resin on to the mould surface prior to the first layer of carbon is all you need to do, IMO.
|