Safety - Which respirator filter to use with epoxy resins?
Safety - Which respirator filter to use with epoxy resins?
Post Reply
Like
3
Safety - Which respirator filter to use with epoxy resins?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ronanobrien
r
ronanobrien
posted 8 Years Ago
ANSWER
HOT
Topic Details
r
Group: Forum Members
Posts: 4,
Visits: 6
Hello,
I am quite new to using resins and am unsure which respirator filter to use when working with epoxy. I am looking to purchase a 3M 6000 series respirator, but when searching which filter i will require as i'm not too sure what the hazards associated with using resins are (and any other safety equipment aside from nitrile gloves). I will link the chart i found below
Any help will be much appreciated
cheers
Ronan
Rrespirator link: .
https://www.3m.co.uk/3M/en_GB/company-uk/3m-products/?N=5002385+8709322+8711017+8711405+8720539+8720550+8720785+8726637+3291100221&rt=rud
3m filter list:
https://www.ucl.ac.uk/~ucapnsz/3M-Selection-Guide.pdf
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Safety - Which respirator filter to use with epoxy resins?
ronanobrien
-
8 Years Ago
Select the epoxy one from the fibreglass section. It shows a 6051 filter. You can get additional particulate filters if you want them.
Warren (Staff)
-
8 Years Ago
Thats great thank you very much! Just wanted to be safe rather than sorry i didn't ask!
ronanobrien
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search