silicon mold and resin kit question
silicon mold and resin kit question
Post Reply
Like
8
silicon mold and resin kit question
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
silverrose
silverrose
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 3
Hi there,
if I want to make a two part mould, do I need a release agent for the silcone rubber and if so which one?
Thanks so much for you time
Emma
Tags
release agent
silicone
two part
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
silicon mold and resin kit question
silverrose
-
14 Years Ago
Silicone are normally self-releasing so the dont need any release agent, except when you want to...
matthieutje65
-
14 Years Ago
Hi Emma, Like matthew says, the only thing silicone really sticks to is silicone and so, if you...
Matt (Staff)
-
14 Years Ago
Sorry to be stupid, but seam line? You mean don't apply it to the first half of the silicone that is...
silverrose
-
14 Years Ago
Hi Emma, Yes, I do mean apply it to the first half of the cured silicone (if you decide to do it in...
Matt (Staff)
-
14 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search