I am doing a lamination process with the EL2 AT30 Slow. I was checking the post-cure instructions on its TDS and I have some questions:
- The post-cure procedure should be applied after the demould time of my resin? Which would be 30h (@25C) + 24h (@Ambient) + 6h (@60C) with post-cure #1.
- Is it a good idea to cool my pot in an ice-bath to increase pot-life and prevent sudden rise in temperature?
- If I am using shrink tape, is it a good idea to use EL160 instead when using a hot-gun? Or the short exposure of the shrink tape to the hot gun will not damage EL2?