Hi Guys, 

Use for bonding carbon fiber with carbon fiber or metal based adhesive Methyl Methacrylate however is missing from my suppliers.
I don't buy Vudu Glu because i live in South America.

What can I use to replace vudu glu (adhesive Methyl Methacrylate) ?