Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Nah that's pretty much it. Obviously you wet it out layer by layer, dont try to put all the layers in and try to wet it out all at once. But you can do many layers in one hit, no need to do stages.
If you want to get rid of some excess resin, you'd go peel ply then a perforated release film and then finally breather cloth. Then as you pull vacuum, the excess resin will squeeze out into the breather so you can peel it off layer. This isn't necessary, you can just use the vacuum to hold things in place.
|