Hanaldo - 8/5/2018 10:16:26 PM
Fillers depend on what you are making. What do you need it to do?

we are mostly making Building Exterior Decorative Product like Pillar, Brackets, Capital, Cornice, Balustrade etc.
Can you tell me whether Marble Powder, Dolomite, Silica powder is a filler?? Pls. give me the name of filler. 

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Fillers depend on what you are making. What do you need it to do?
ATUL SHAH
A
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 5, Visits: 10
ATUL SHAH - 8/5/2018 12:38:26 PM
drippy - 8/4/2018 3:46:10 PM
ATUL SHAH - 8/4/2018 6:02:42 AM
WE ARE INTO CUSTOM FRP MOLDING BUSINESS. WE USE ORTHO. BASE POLYESTER RESIN. WHAT IS ADVANTAGE USING ISO BASE POLYESTER RESIN?  

This is a good read if you want to learn about the difference in resins. Granted this is pretty basic but gives you an idea
http://www.nzfibreglass.co.nz/2015/images/differences%20between%20resins.pdf

do you know anything about filler used in the system/process?  

what kind of filler used?? do you make any product for FRP Industry?? you can visit www.grpgrc.com our website 

ATUL SHAH
A
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 5, Visits: 10
drippy - 8/4/2018 3:46:10 PM
ATUL SHAH - 8/4/2018 6:02:42 AM
WE ARE INTO CUSTOM FRP MOLDING BUSINESS. WE USE ORTHO. BASE POLYESTER RESIN. WHAT IS ADVANTAGE USING ISO BASE POLYESTER RESIN?  

This is a good read if you want to learn about the difference in resins. Granted this is pretty basic but gives you an idea
http://www.nzfibreglass.co.nz/2015/images/differences%20between%20resins.pdf

do you know anything about filler used in the system/process?  

drippy
drippy
Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)
Group: Forum Members
Posts: 32, Visits: 388
ATUL SHAH - 8/4/2018 6:02:42 AM
WE ARE INTO CUSTOM FRP MOLDING BUSINESS. WE USE ORTHO. BASE POLYESTER RESIN. WHAT IS ADVANTAGE USING ISO BASE POLYESTER RESIN?  

This is a good read if you want to learn about the difference in resins. Granted this is pretty basic but gives you an idea
http://www.nzfibreglass.co.nz/2015/images/differences%20between%20resins.pdf

Edited 7 Years Ago by drippy
ATUL SHAH
A
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 5, Visits: 10
WE ARE INTO CUSTOM FRP MOLDING BUSINESS. WE USE ORTHO. BASE POLYESTER RESIN. WHAT IS ADVANTAGE USING ISO BASE POLYESTER RESIN?  
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search