I have a 2 piece mould, that needs to be butt jointed together, I was just wondering what method you guys would recommend to bond? To start with I will be using fibreglass to make the parts. I was thinking maybe some gel coat...but it would need to be pretty thick to make sure it didnt all run out of the mould... 