Casting letters on epoxy carbon


Author
Message
Carbon Tuner
Carbon Tuner
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 104, Visits: 422
Did you end up trying this? Any Pics?



If Brute Force Isn''''t working your not using enough...
darknight7777777
darknight7777777
Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)
Group: Forum Members
Posts: 7, Visits: 254
Hi,

The carbon is about 1.5mm thick but the cast letters max 3-4mm thick and 5cm width by 20cm length.

thanks
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
In my opinion I don't see any problem... 

maybe sand the carbon just a little bit with a 600grid sandpaper, to have a better bond, and clean it with some cleaning alcohol to remove any sanding dust befor casting.
I don't know how the casting resin is made but remember; polyester won't bond to epoxy..., polyurethane casting resins should be ok I guess
How thick will the part be in casting resin? to have a very clear casting you should do small layers at the time not to overheat your resin, causing some cracks and colourdistortion.

Hope this might help you a little further...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




darknight7777777
darknight7777777
Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)Supreme Being (189 reputation)
Group: Forum Members
Posts: 7, Visits: 254

I am planning to cut out a couple of letters out of a epoxy carbon plate and then hoping to pour water clear casting resin to fill letters.

Is it possible or would there be any issues. 

Would the casting resin bond with the carbon plate or would it need extra bonding to keep the letters from coming out.