ants87ss
a
ants87ss
posted 8 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 4,
Visits: 50
So my first shot at making a mold. I know what I did, gelcoat was too hot before I mixed it and I also let the plug sit in the sun for a while. My question is, can this be saved? Or should I just start over
Edited
8 Years Ago by
ants87ss
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Uh oh. Need help!( pic added)
ants87ss
-
8 Years Ago
It's hard to tell from the pic, but I can't really see a whole lot wrong with it other than the poor coverage. If that's the only problem then just do another coat of gelcoat and carry on. If there'...
Hanaldo
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search