			            As you even mentioned, in an ideal world you would test it.
 However  it is unlikely you will have any problems as long as you prepare things properly.  You want to ensure the paint is fully cured  before starting.  A good key with sandpaper at 120-240 grit will provide a good surface for the resin to bond to.  Although take care not to go through the paint totally .    Ensure you give the door a final clean before coating with resin and you should be good  to go.
 
 