Good morning, I am using Axson Epolam 2017 General Purpose Epoxy Resin System - Lloyds Approved with 420 biaxial fiberglass. I am using easy composites vacuum bagging materials, I am finding small leaks where the bagging tape is allowing air through the seal onto of the epoxy resin. When laying up the fibreglass I have used peel ply in hopes to remove the tacky film left behind. I have also tried sanding. and of course washing down with acetone. The leaks are minute and barely dectable with leak detector. ANY suggestion on how to get a better seal?
|