The Yellow filleting wax you see can be used for room temperature processes including vacuum bagging and infusion. Occasionally people will make temporary mould repairs or changes using the wax. Resin does not stick to it so it can be easily scraped off after the resin has cured.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|