cvasilliou - 6/1/2018 5:09:02 PM
lets say i just made a carbon fibre mold(a part of cars front wing for example).i would like to know for how long i will be able to use this mold in my car.

and lets say i used another carbon fiber mold(steering wheel) and after a year i realise i cant make any development in this part(so i dont have to make a new mold).will i be able to use it after all this time and offers me the same results?

Still making bits out of moulds 30 yrs old
Grp wet lay moulds I put a gel in them to protect the surface
Pre preg carbon moulds just store on the shelf

cvasilliou
c
Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)
Group: Forum Members
Posts: 16, Visits: 102
lets say i just made a carbon fibre mold(a part of cars front wing for example).i would like to know for how long i will be able to use this mold in my car.

and lets say i used another carbon fiber mold(steering wheel) and after a year i realise i cant make any development in this part(so i dont have to make a new mold).will i be able to use it after all this time and offers me the same results?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search