Advise please to make a good repair to a Moses kitesurfing carbon fibre hydrofoil mast


Advise please to make a good repair to a Moses kitesurfing carbon fibre hydrofoil mast
Author
Message
rev
r
rev
posted 7 Years Ago HOT
Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)
Group: Forum Members
Posts: 1, Visits: 9
Hi all

 I have made some small damage to the trailing edge to the mast 3mm deep by 20mm long

Its on the trailing edge which is very thin approx. 2mm
I'm looking for a good atheistic repair solution to this.

What materials can you sugest please that will be jet black in colour to match up with carbon fibre

Ive never worked with carbon fibre before

Thanks in advance