Group: Forum Members
Posts: 550,
Visits: 27K
|
Personally I use "high gloss" release agent, sold by hp-textiles in Germany. Incredible easy release, super fast drying, polishable with a soft cloth, useable for hight temperatures and highly efficient. And as a bonus it is water based, wich makes removing build up release agent super easy, although I never had to do it. But still, it's semipermant, unlike pva, doesn't build a film, and gives a brilliant surface replication. But easylease from easycomposites seems to have similar propertys, except it isn't water based.
|