Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Jake, Welcome to the forum!

You are right that the Permabond 515 would be suitable for this application, we have supplied this to many home frame-builders and always had good reports, the small degree of flex that it can handle it ideal for the highly shocked joints of a frame. If this is a repair you should really have to worry about corrosion issues the inside to the contacting tube will probably have been insulated from the Aluminium with a layer of glass cloth, not all frame manufacturers bother with this; Galvanic corrosion between a typical carbon laminate and aluminium is usually negligible and rarely results in failure.

As for preparation, simply key both faces with a coarse sand-paper (80 grit), degreasing both before and after, and then bond the joint as normal, leave the adhesive to fully cure; allow at least 48hrs somewhere warm before riding. There really shouldn't be much more to it than that.

Paul Statham
Easy Composites / Carbon Mods - Technical
jake
jake
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 4
Hi,

Apologies if this has been covered, a search didn't throw anything up.

Can anyone recommend a product to bond carbon fibre tubes into aluminium lugs as part of repairing a bicycle frame of the same construction- so i would assume a structural adhesive is needed. Obviously high strength is needed, and presumably a very small amount of flex? maybe one of the permabonds (et515?)- not sure which one? I am also concerned about corrosion of the aluminium- is this a necessary worry, and are there any mitigations?

Supplementary question- i'd like to sand back refinish the carbon fibre- would the epoxy coating resin do the trick? does it require lacquering afterwards for a lovely shiny finish?

Thanks for any help!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search