Not overly familiar with PETG, but if it similar to acrylic then I'd be careful as epoxy will actually bond somewhat to acrylic. Epoxy won't attack anything as there's no solvents in it, but it will stick to some plastics. Not super well, but enough to make life difficult. Its likely that the plastics you saw in the videos were polypropylene rather than acrylic.
As for the clay, I'm familiar with Monster Clay and it should work fine.
|