I started using a fresh container of GlassCast 10 about 10 days ago using about 2/3rds of the contents.

Today, when I went to use the remaining epoxy, I found is was severely crystallised and not pourable.

There has been no contamination with the hardner.

What has gone wrong, or is there a very short shelf life once the container is opened?