Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Mould repair of pinholes
Mould repair of pinholes
Post Reply
Like
3
Mould repair of pinholes
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
SHaas
S
SHaas
posted 7 Years Ago
ANSWER
HOT
Topic Details
S
Group: Forum Members
Posts: 46,
Visits: 383
Hi everybody,
I searched the forum and already found some interesting threads about this theme but I have an additional question.
I already tried about 4 moulds with high epoxy temperature gelcoat (EM160 from EC) but every time I have some tiny pinholes on the surface as you may see in the photo on the right. I do not know where the mistake is but now I am going to try a repair instead of doing another mould. So I was wondering if it is possible to get away with the pinholes by using the S120 board sealer? Anyone with experience in this? I read a lot about using it to epoxy modelboard but I think this has no pinholes. After all I think the pinholes are too small to fill up with new epoxy and get a good key!?
The left picture shows the only one large hole in my mould. This is too big for S120 for sure, but do you think it is necessary to repair it after all because it is not on the surface of the finished part. Or will this hole steal too much resin from my prepreg so that there will be imperfections on the surface because of that? If I have to repair it with some additional gelcoat, will there be no problem becaus I cannot make a key on the surface!?
And my last question: The surface of the original part has a matt finish. But I want the carbon to be high gloss. So usually I would polish my mould. But what is when using the board sealer all over the mould? Would this be enough to get a high gloss if you follow the TDS and use about 5 layer, sand it with 1200 grit and put a final layer on?
Thanks a lot for your help guys!
Edited
7 Years Ago by
SHaas
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Mould repair of pinholes
SHaas
-
7 Years Ago
The pinholes are trapped air. The bigger ones should be easy to fill in. The tiny ones you can sand back and recoat or try wiping over with gel to fill them. Sanding back is usually more successful.....
Warren (Staff)
-
7 Years Ago
Thanks Warren! Can you perhaps give me also some infos about my S120 board sealer questions?
SHaas
-
7 Years Ago
You will unlikely fill big pinholes like that, more for surface fine porosity, dullness, fine scratches etc over the whole surface where a recoating all over would be beneficial.
Warren (Staff)
-
7 Years Ago
What about this? And my last question: The surface of the original part has a matt finish. But I want the carbon to be high gloss. So usually I would polish my mould. But what is when using the boar...
SHaas
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search